Despriciton: Oxidation and hot corrosion behaviour of Nimonic- 75 Oxidation and hot corrosion behaviour of Nimonic- 75 superalloy K S Sreenivas V M Radhakrishnan Metallurgical Engineering Department,Indian Institute of Technology-Madras,Chennai 600 036,India Received 7 February 1997; accepted 5 June 1998 Experiments were carried out to study the oxidation and hot co...